Steel name: WELL-TEN80S(43)
Diagram No.: 570
Type of diagram: CCT
Chemical composition in weight %: 0.074% C, 0.57% Si, 1.35% Mn, 0.009% P,
0.003% S, 0.06% Ni, 0.12% Cu, 0.92% Cr, 0.52% Mo, 0.06% V, 0.026% Ti.
Note: Calculated welding CCT diagram. Austenitizing temperature: 1623 K,
30 seconds.
Source: NIMS Database, 2007, Japan.
Price: 30.00 US $