Steel name: Carpenter 20Nb-3 Stainless Steel Strip
Diagram No.: 2970
Type of diagram: TTS
Chemical composition in weight %: 0.036% C, 0.23% Mn, 0.38% Si, 0.020% P, 0.004% S,
33.70% Ni, 19.76% Cr, 2.25% Mo, 3.14% Cu, 0.79% Nb.
Note: Precipitation diagram. Time-temperature sensitization and intergranular corrosion.
Treatment: Mill annealed (941
oC) material was sensitized in the temperature range
566-885
oC for 30 min to 48 h prior to intergranular corrosion testing.
Source: M. Henthorne, T.A. DeBold, "Intergranular Corrosion Resistance of Carpenter
20Nb-3", Corrosion, Vol.27, No.6, June 1971, p.255.
Price: 25.00 US $