18Cr-2Mo-Ti Stabilized Ferritic Stainless Steel
  Steel name: 18Cr-2Mo-Ti Stabilized Ferritic Stainless Steel
  Diagram No.: 2908
  Type of diagram: TTS
  Chemical composition in weight %: 0.023% C, 0.33% Mn, 0.16% Si, 0.019% P, 0.012% S,
  0.33% Ni, 17.15% Cr, 2.23% Mo, 0.04% Cu, 0.05% Co, 0.61% Ti.
  Note: Precipitation diagram. Time-temperature sensitization and intergranular corrosion.
  Influence of aging treatment on intergranualar corrosion behavior.
  See the diagram No. 2907.
  Source: T.M.Devine, A.M. Ritter, B.J. Drummond, "Influence of Heat Treatment on the
  Sensitization of 18Cr-2Mo-Ti Stabilized Ferritic Stainless Steel", Metallurgical
  Transactions A, Vol.12A, ASM, December 1981, p.2063.