Steel name: 18Cr-2Mo Ferritic Stainless Steel
Diagram No.: 2892
Type of diagram: TTE
Chemical composition in weight %: 0.013% C, 0.49% Mn, 0.27% Si, 0.019% P, 0.013% S,
17.40% Cr, 2.00% Mo, 0.0095% N, 0.35% Nb.
Note: Embrittlement diagram. Temper embrittlement. Embrittlement of stainless steel.
Time-temperature diagram of age hardening of steel investigated. The points indicated
the time necessary to increase the hardness by ten points HV 10.
Source: J. Grobner, R.F. Steigerwald, "Effect of Cold Work on the 475
oC (885
oF)
Embrittlement of 18Cr-2Mo Ferritic Stainless Steels", Transactions AIME, Vol.29,
July 1977, p.17.
Price: 30.00 US $
Buy Online
We sell's software, not a steels
Hardenability diagrams of steels
Tempering diagrams of steels