Alloy Steel
  Steel name: Alloy Steel
  Diagram No.: 2886
  Type of diagram: TTE
  Chemical composition in weight %: 0.44% C, 1.64% Mn, 0.06% Si, 0.029% P, 0.022% S,
  1.84% Ni, 1.64% Cr, 0.40% Mo, 0.15% Cu.
  Note: Embrittlement diagram. Temper embrittlement. Austenitizing temperature: 900oC
  (1650oF). Grain szie: 6. IT diagram. See the diagrams No. 2887 and No. 2888.
  Source: W.S. Pellini, B.R. Queneau, "Developmnet of Temper Brittlness in Alloy Steel",
  Transactions of the ASM, Vol.39, ASM, 1947, p.139.