Steel name: SAE 3140
Diagram No.: 2877
Type of diagram: TTE
SAE designation: 3140
Chemical composition in weight %: No data.
Note: Embrittlement diagram. Temper embrittlement. Treatment: Specimens previously
austenitized at 900
oC (1650
oF) for 1 h and water quenched. Specimens treated at
660
oC and below were also given a prior temper 1 h at 675
oC and water quenched;
plotted times for 675 and 700
oC are adjusted accordingly.
Source: L.D. Jaffe, D.C. Buffum, "Upper Nose Temper Embrittlemnet of a Ni-Cr Steel",
Transactions AIME, Vol.209, January 1957, p.8.