SAE 4047 Steel
  Steel name: SAE 4047
  Diagram No.: 2876
  Type of diagram: TTE
  SAE: 4047
  Chemical composition in weight %: 0.48% C, 0.83% Mn, 0.28% Si, 0.019% P, 0.015% S,
  0.14% Ni, 0.13% Cr, 0.25% Mo.
  Note: Embrittlement diagram. Temper embrittlement. Austenitizing temperature: 815 oC
  (1500 oF). Grain size: 7. Figures beside points represent increase in transition
  temperature (oF) based on transition temperatures of specimens tempered at 1260 oF
  for 5 s. Figures in parentheses are the average hardness of the speicmens in that series.
  Source: G. Bhat, J.F. Libsch, "Isoembrittlement in Chromium and Molybdnum Alloy Steels
  During Tempering", Transcations AIME, Vol.203, February 1955, p.330.

  Price: 25.00 US $