0.44 C Steel
  Steel name: 0.44 C Steel
  Diagram No.: 2761
  Type of diagram: TTT
  Chemical composition in weight %: 0.44% C, 0.50% Mn, 0.18% Si, 0.42% Ni, 0.22% Cr.
  Note: Influence of applied pressure on transfomation. Structural steel. Austenitizing
  temperature: 980 oC (1800 oF). Grain size: 1-3.
  See the diagrams No. 2762 and No. 2763.
  Source: T.G. Nilan, "Morphology of Austenite Decomposition at High Pressure",
  Transactions of The Metallurgical Society of AIME, Vol.239, June 1967, p.898-909.

  Price: 25.00 US $
  Buy Online


Terms of Use. Copyright © 2007 by Henrik Kaker. All Rights Reserved.