Steel name: 13CrMo4-4 Steel
Diagram No.: 2711
Type of diagram: CCT
Mat. No. (Wr. Nr.) designation: 1.7335
DIN designation: 13CrMo 4 4
Chemical composition in weight %: 0.11% C, 0.56% Mn, 0.30% Si, 0.015% P, 0.015% S,
0.07% Ni, 0.84% Cr, 0.48% Mo, 0.01% V, 0.002% Al, 0.011% N.
Note: Alloy steel. Austenitizing temperature: 945
oC for 8 min.
Source: R. Petri, et al., "During Cooling-Resistant Tube Stels After Austenitising Part 1:
Chromium-Molybdenum Steels", Arch. Eisenhuttenwes., Vol.51, No.8, 1980, p.355-360.