Steel name: C-Mn Steel
Diagram No.: 2679
Type of diagram: CCT
Chemical composition in weight %: 0.11% C, 1.99% Mn, 0.29% Si, 0.012% P, 0.009% S.
Note: Structural steel. Austenitizing temperature: 1200
oC (2192
oF) for 10 min.
PF-polygonal ferrite, P-pearlite, AF-acicular ferrite, B-bainite, PP-pseudopearlite,
M
2nd-martensite second phase, M
s-transformation start temperature of martensite,
M
's-transformation start temperature of martensite second phase.
See the diagrams
No. 2676,
No. 2677 and
No. 2678.
Source: Jye-Long Lee, et al., "Transformation Processes and Products for C-Mn Steels
during Continuous Cooling", Materials Science and Technology, Vol.5, July 1989,
p.674-681.