Low-Carbon Low-Alloy High-Strength Steel
  Steel name: Low-Carbon Low-Alloy High-Strength Steel
  Diagram No.: 2615
  Type of diagram: TTT
  Chemical composition in weight %: 0.12% C, 0.83% Mn, 0.30% Si, 0.004% P, 0.005% S,
  0.30% Cu, 1.11% Ni, 0.53% Cr, 0.49% Mo, 0.03% V, 0.031% sol. Al.
  Note: Low-Carbon Low-Alloy High-Strength Steel. Austenitizing temperature:
  1200oC (2192oF) for 5 min. See the diagrams No. 2614, No. 2616 and No. 2617.
  Source: Yasuya Ohmori, et al., "The Bainite in Low Carbon Low Alloy High Strength Steel",
  Transactions ISIJ, Vol.11, 1971, p.250-259.