Steel name: W2 Tool Steel
Diagram No.: 2571
Type of diagram: TTT
Chemical composition in weight %: 0.95% C, 0.20% V.
Note: Tool steel. Austenitizing temperature: 795
oC (1450
oF). Grain size: 9-1/2.
Source: Data Sheet, Crucible Steel Co. of America, December 1947, as published in
Atlas of Isothermal Transformation and Cooling Transformation Diagrams, ASM, 1977.
Price: 25.00 US $