T2 Tool Steel
  Steel name: T2 Tool Steel
  Diagram No.: 2544
  Type of diagram: TTT
  Chemical composition in weight %: 0.85% C, 4.00% Cr, 0.75% Mo, 2.10% V, 18.50% W.
  Note: Tool steel. Austenitizing temperature: 1285 oC (2350 oF).
  Source: Data Sheet, Crucible Steel Co. of America, December 1947, as published in
  Atlas of Isothermal Transformation and Cooling Transformation Diagrams, ASM, 1977.