403 Stainless Steel
  Steel name: 403 Stainless Steel
  Diagram No.: 2526
  Type of diagram: TTT
  Chemical composition in weight %: 0.15% C, max.1.00% Mn, max.0.50% Si,
  max.0.04% P, max.0.03% S, 11.50-13.00% Cr.
  Note: Stainless steel. Austenitizing temperature: 890 oC (1800 oF).
  Source: Data Sheet, Crucible Steel Company of America, October 1948, as published in
  Atlas of Isothermal Transformation and Cooling Transformation Diagrams, ASM, 1977.

  Price: 25.00 US $