Croloy 7 Steel
  Steel name: Croloy 7
  Diagram No.: 2491
  Type of diagram: TTT
  Chemical composition in weight %: 0.12% C, 0.53% Mn, 0.55% Si, 0.015% P, 0.036% S,
  0.07% Ni, 7.50% Cr, 0.45% Mo.
  Note: Alloy steel. Austenitizing temperature: 1015 oC (1860 oF) for 40 min. Grain size: 4-5.
  Source: Intermediate Croloy Steels, Babcock & Wilcox.