Steel name: 0.38% C-V-Cr-Mo
Diagram No.: 2231
Type of diagram: CCT
Chemical composition in weight %: 0.38% C, 0.87% Mn, 0.18% Si, 0.008% S, 0.027% P,
1.54% Cr, 0.01% Ni, 0.63% Mo, 0.27% V
Steel group: Quenched and tempered engineering steel, vanadium steel
Note: Austenitizing temperature: 970
oC in 3 minutes and holding time: 15 minutes.
Source: Atlas zur Warmebehandlung der Stahle, Max-Plank Institut fur Eisenforschung, 1958,
as published in Atlas of Continuous Cooling Transformation Diagrams for Vanadium Steels,
Vanitec, England, June 1985