Steel name: 0.12% C-0.85% Mn-0.3% Si-1.4% Ni-0.7% Cr
Diagram No.: 2069
Type of diagram: CCT
Chemical composition in weight %: 0.12% C, 0.87% Mn, 0.35% Si, 1.44% Ni, 0.76% Cr.
Note: Molybdenum steel. Austenitizing temperature: Ac
3 + 30
oC (54
oF) for 12 min.
Source: Witold W. Cias, Austenite Transformation of Ferrous Allloys, Climax Molybdenum
Company, Greewich CT, USA.
Click the image to enlarge the diagram.