Steel name: 0.10% C-0.7% Mn-0.3% Si-0.3% Cr-0.25% Mo-B
Diagram No.: 2018
Type of diagram: CCT
Chemical composition in weight %: 0.11% C, 0.70% Mn, 0.35% Si, 0.28% Cr,
0.0045% B, 0.25% Mo.
Note: Molybdenum steel. Austenitizing temperature: Ac
3 + 30
oC (54
oF) for 12 min.
Source: Witold W. Cias, Austenite Transformation of Ferrous Allloys, Climax Molybdenum
Company, Greewich CT, USA.