Steel name: 0.36% C-0.8% Mn-0.3% Si-0.7% Ni-0.82% Mo
Diagram No.: 1999
Type of diagram: CCT
Chemical composition in weight %: 0.36% C, 0.75% Mn, 0.29% Si, 0.72% Ni, 0.82% Mo.
Note: Molybdenum steel. Austenitizing temperature: Ac
3 + 30
oC (54
oF) for 20 min.
Source: Witold W. Cias, Austenite Transformation of Ferrous Allloys, Climax Molybdenum
Company, Greewich CT, USA.
Price: 30.00 US $