Steel name: 0.10% C-0.70% Mn-0.30% Si-3.00% Ni-0.55% Mo-B
Diagram No.: 1992
Type of diagram: CCT
Chemical composition in weight %: 0.11% C, 0.74% Mn, 0.34% Si, 3.03% Ni,
0.55% Mo, 0.0057% B.
Note: Molybdenum steel. Austenitizing temperature: Ac
3 + 30
oC (54
oF) for 12 min.
Source: Witold W. Cias, Austenite Transformation of Ferrous Allloys, Climax Molybdenum
Company, Greewich CT, USA.