0.10% C-0.70% Mn-0.30% Si-1.40% Ni-B Steel
  Steel name: 0.10% C-0.70% Mn-0.30% Si-1.40% Ni-B
  Diagram No.: 1987
  Type of diagram: CCT
  Chemical composition in weight %: 0.097% C, 0.69% Mn, 0.31% Si, 1.45% Ni,
  0.0048% B.
  Note: Molybdenum steel. Austenitizing temperature: Ac3 + 30 oC (54 oF) for 12 min.
  Source: Witold W. Cias, Austenite Transformation of Ferrous Allloys, Climax Molybdenum
  Company, Greewich CT, USA.