0.37% C-0.50% Mn-0.30% Si-0.19% Mo Steel
  Steel name: 0.37% C-0.50% Mn-0.30% Si-0.19% Mo
  Diagram No.: 1965
  Type of diagram: CCT
  Chemical composition in weight %: 0.36% C, 0.50% Mn, 0.32% Si, 0.19% Mo.
  Note: Molybdenum steel. Austenitizing temperature: 843 oC (1550 oF) for 20 min.
  Source: Witold W. Cias, Austenite Transformation of Ferrous Allloys, Climax Molybdenum
  Company, Greewich CT, USA.

  Price: 25.00 US $