Steel name: 206
Diagram No.: 1929
Type of diagram: CCT, TTT
Chemical composition in weight %: 0.325% C, 0.54% Mn, 0.22% Si, 1.103% Cr,
0.63% Mo, 0.17% V.
Note: Tool steel. Austenitizing temperature: 850
oC (1562
oF) for
30 min.
Ac
1: 736
oC, Ac
3: 858
oC.
Diagram Description: Duree de chauff. - Time to temperature, Duree d'austenit. - Time
while austenite, Temperature d'austenit. - Austenitizing temperature, Grain austenit.
- Austenite grain size, Duree du refroidissement entre 800 et 500
oC - min - Cooling time
between 800 and 500
oC minutes , Durete Vickers (30 kg) - Vickers hardness
(30 kg load), kg/mm
2 - Units for HV test.
The x-axis is not a simple plot of time and, therefore, cooling curves are not
superimposed over diagrams. Instead, the x-axis plots the time required to cool from
800 to 500
oC, which is related to the cooling rate. Because of this manner of graphical
presentation, the transformation is given along vertical lines, rather the usual
superimposed cooling curves. Also because of this construction, it is possible to plot
room tmeperature hardness as a function of the 'half-cooling' time with a single curve.
Source: M. Economopoulos, N. Lambert, L. Habraken, Diagrammes de Transformation
des Aciers Fabriques dans le Benelux, Centre National de Recherches
Metallurgiques, Brussels, Belgium, 1967.