Steel name: 16 NC 6
Diagram No.: 1721
Type of diagram: TTT
Mat. No. (Wr. Nr.): 1.5919
DIN: 15CrNi6
AFNOR NC: 16 NC 6
Chemical composition in weight %: 0.15% C, 0.55% Mn, 0.30% Si, <0.010% S, 0.013% P
1.38% Ni, 0.82% Cr, 0.09% Mo, 0.11% Cu.
Note: Alloy special structural steel. Austenitizing temperature: 900
oC (1652
oF) for
30 min. Grain size: 8-11.
Ac
1: 740
oC, Ac
3: 835
oC, M
s: 395
oC.
Source: Courbes de Transformation des Aciers de Fabrication Francaise, IRSID, Paris,
France, 1974.