Steel name: 2.5% Ni-Cr-Mo Medium Carbon Steel
Diagram No.: 1578
Type of diagram: TTT
B.S.: En 25
Chemical composition in weight %: 0.32% C, 0.27% Si, 0.56% Mn, 0.012% S, 0.018% P,
2.37% Ni, 0.74% Cr, 0.51% Mo.
Note: Structural steel, medium carbon steel. Austenitizing temperature: 835
oC.
As quenched grain size: 7 & 8.
McQuaid grain size: 3-4.
Hardness values in bold figures are shown of the fully transformed steel; the values in
italics represent structures developed by holding at the selected temperatures for 24
hours and then quenching to room temperature.
Source: George F. Vander Voort, Atlas of Time-Temperature Diagrams for Irons and
Steels, ASM International, USA, 1991, p.87.
Price: 25.00 US $