0.15C-1Cr-0.9Mo-0.2V Steel
  Steel name: 0.15C-1Cr-0.9Mo-0.2V
  Diagram No.: 1364
  Type of diagram: CCT
  Chemical composition in weight %: 0.13% C, 0.38% Si, 0.63% Mn, 0.016% P, 0.012% S,
  0.95% Cr, 0.86% Mo, 0.07% Ni, 0.19% V.
  Note: Tool steel. Austenitizing temperature: 960oC.
  Holding time: 15 min, brought up to temperature in 5 min.
  Source: A. Rose, F. Wever, W. Peter, Atlas Zur Warmebehandlung Der Stahle,
  Verlag Stahleisen, Dusseldorf, Germany, 1954, 1956, 1958.

  Price: 30.00 US $