0.4C-1.8Mn Steel
  Steel name: 0.4C-1.8Mn
  Diagram No.: 1360
  Type of diagram: CCT
  Chemical composition in weight %: 0.42% C, 0.27% Si, 1.82% Mn, 0.026% P, 0.018% S.
  Note: Unalloyed carbon steel. Austenitizing temperature: 860oC.
  Holding time: 7 min, brought up to temperature in 3 min.
  Source: A. Rose, F. Wever, W. Peter, Atlas Zur Warmebehandlung Der Stahle,
  Verlag Stahleisen, Dusseldorf, Germany, 1954, 1956, 1958.